Description
- According to DIN 29453
Art.-No. 5490 25:
- 3 metal alloy: 74 % Pb (lead) , 25 % Sn (tin) , 1 % Sb (antimony)
- Working temperature: +190 °C to +250 °C
Art.-No. 5490 33:
- 3 metal alloy: 67 % Pb (lead), 33 % Sn(tin), 0,5 % Sb (antinomy)
- working temperature: +250 °C to + 350 °C
Art.-No. 5490 40:
- 3 metal alloy: 59.5 % Pb (lead), 40% Sn (tin), 0.5 % Sb (antimony)
- Working temperature: +200 °C to +350 °C
Art.-No. 5490 50:
- 3 metal alloy: 50 % Pb (lead), 50 % Sn (tin), 0,5 % Sb (antinomy)
- Working temparature: +250 °C to +300 °C
Art.-No. 5490 60:
- 3 metal alloy: 40 % Pb (lead), 60 % Sn (tin), 0,5 % Sb (antinomy)
- Working temparature: +220 °C to +350 °C